Brand Name : JIN LAI
Model Number : High Alloy Stainless Steel
Certification : ISO
Place of Origin : CHINA
MOQ : 5 tons
Price : negotiable based on the quantity
Payment Terms : T/T, Western Union, L/C
Supply Ability : 3000 tons per month
Delivery Time : within 15 days
Packaging Details : standard seaport packing or as customers' request
Standard : ASTM, AISI, DIN, EN, GB, JIS
Material : stainless steel
Length : 1000-6000mm
Width : 150mm-2500mm
Surface : BA/2B/NO.1/NO.3/NO.4/8K
Edge : Slit edge or mill edge
Technic : cold rolled/hot rolled
Port : Shanghai
Hastelloy C22, also known as alloy C22, is a versatile austenitic nickel-chromium-molybdenum-tungsten alloy with enhanced resistance to pitting, crevice corrosion and stress corrosion cracking. The high chromium content provides good resistance to oxidizing media while the molybdenum and tungsten content give good resistance to reducing media. This nickel steel alloy also has excellent resistance to oxidizing aqueous media including wet chlorine and mixtures containing nitric acid or oxidizing acids with chlorine ions. Other corrosives Hastelloy C-22 has resistance to are oxidizing acid chlorides, wet chlorine, formic and acetic acids, ferric and cupric chlorides, sea water, brine and many mixed or contaminated chemical solutions, both organic and inorganic. This nickel alloy also offers optimum resistance to environments where reducing and oxidizing conditions are encountered in process streams. This is beneficial in multi- purpose plants where such “upset” conditions occur frequently.
This nickel alloy resists the formation of grain-boundary precipitates in the weld heat-affected zone, thus making it suitable for most chemical process applications in the as-welded condition.
Alloy C-22 should not be used in service temperatures above 1250° F due to the formation of detrimental phases which form above this temperature.
characteristics
Chemical Composition, %
|
C |
Cr |
Co |
Fe |
Mn |
Mo |
Ni |
P |
Si |
S |
W |
V |
|---|---|---|---|---|---|---|---|---|---|---|---|
| .010 max | 20-22.5 | 2.5 max | 2.0-6.0 | .50 max | 12.5-14.5 | Balance | .02 max | .08 max | .02 max | 2.5-3.5 | .35 max |
Application
Fabrication of Hastelloy C-22
Although ductile enough to be formed by cold working, intermediate annealing may be necessary due to work hardening. Forging should be performed between 1750-2050° F followed by rapid cooling. Annealing can be performed at a temperature range between 2020-2150° F followed by a rapid quench. Cooling at an accelerated rate avoids the formation of detrimental phases which form between 1400-1800° F. Welding can be done by gas tungsten-arc, gas metal-arc and shielded metal-arc processes.
ASTM Specifications
|
Pipe Smls |
Pipe Welded |
Tube Smls |
Tube Welded |
Sheet/Plate |
Bar |
Forging |
Fitting |
|---|---|---|---|---|---|---|---|
| B622 | B619 | B622 | B626 | B575 | B574 | B564 | B366 |
Mechanical Properties
Typical Room Temperature Tensile Properties of Annealed Material
|
Product Form |
Tensile (ksi) |
.2% Yield (ksi) |
Elongation % |
Hardness (HRb) |
|---|---|---|---|---|
| Plate (.25”-1.75”) | 112 | 53 | 62 | 89 |
| Sheet (.038”-.15”) | 122 | 63 | 54 | 93 |
| Bar (.50”-5.50”) | 115 | 55 | 60 | 89 |
|
|